Home / Chemicals / By application
Chemistry · by application

Start from the contamination. Then the part.

The jobs the range is documented for, what is on the part, the component it is on, what that is made of, and the chemical that takes it off. Search the part by name, or pick a sector. Every dose and temperature on this page is the one printed on that product’s current technical data sheet: the trial sets your exact process values against your soil. Working out what that means in litres? Use the dosage calculator.

30 applications

Aerospace MROSpray cabinet

Oils and fingerprints off cadmium-plated parts

Comes offoils·coolants·fingerprints·particulate
Parts arecadmium plating·copper alloys·brass·aluminium
Also coverscadmium·copper plated·plated part·sensitive metal
Run it at3–15% (typ. 5%)·49–82 °C
AquaVantage 1696 GD →
Aerospace MROImmersion / ultrasonic

Carbon and grease off engine and turbine parts

Comes offoils·grease·carbon·buffing compound·coolants
Parts aresteel·aluminium·titanium·nickel alloys·cadmium plating
Also coversturbine blade·compressor·engine part·airframe part
Run it at7–30% (typ. 10%)·54–77 °C
AquaVantage 815 GD →
Aerospace MROSpray cabinet

Oils and coolants off precision components

Comes offoils·coolants·particulate·buffing compound
Parts arealuminium·steel·titanium·magnesium
Also coversspray cabinet·cabinet washer·precision part
Run it at3–15% (typ. 5%; 5% min on aluminium)·49–77 °C
AquaVantage 1990 GD →
Alloy and wheel refinishingImmersion / ultrasonic

Paint and lacquer off alloy wheels

Comes offpaint·powder coat·lacquer·baked finishes
Parts arealuminium·zinc
Also coversalloy wheel·wheel·rim·powder coat
Run it at10% v/v of the mixed system·40–70 °C
AlloySystem →

Not safe on magnesium.

Carbon, paint and rust off ferrous engine parts

Comes offbaked carbon·paint·rust·scale·grease
Parts arecast iron·carbon steel·steel
Also coversengine component·cylinder head·manifold·decarbonise
Run it at10–30% v/v (typ. 25%)·60–80 °C
MetalTek 100 →

Ferrous only. Aluminium, zinc and tin are attacked rapidly and glass is etched, a single alloy part in the basket will be lost.

Diesel and DPF regenerationImmersion / ultrasonic

Ash out of DPF filters and cans

Comes offcalcium ash·zinc phosphate·magnesium oxides·mineral ash
Parts arecordierite·silicon carbide·stainless steel
Also coversDPF·diesel particulate filter·ash·regeneration·filter can
Run it atneat, no dilution·ambient–50 °C
RegeniK →

Ferrous and ceramic only. Aluminium, zinc, magnesium, cadmium, tin and solder are excluded, and copper, brass and bronze can suffer stress-corrosion cracking.

Engine reconditioningImmersion / ultrasonic

Baked carbon off cylinder heads and blocks

Comes offbaked carbon·oils·grease·gasket residue
Parts arecast iron·aluminium·steel
Also coverscylinder head·engine block·crankcase
Run it at5–30% (typ. 10%)·54–77 °C
AquaVantage 815 QR-NF →

Keep copper, brass and plastics out of this bath.

Engine reconditioningImmersion / ultrasonic

Varnish and carbon off valve bodies

Comes offvarnish·oils·carbon·fuel residues
Parts arealuminium·steel
Also coversvalve body·carburettor·gearbox·automatic transmission
Run it at10–20% v/v (typ. 15%)·40–60 °C
Desludge →

Check the castings first. The bath runs at pH 13 and zinc, galvanised, magnesium and soft solder are attacked, a zinc die-cast body must not go in.

Engineering and maintenanceImmersion / ultrasonic

Mill scale and rust off steel stock

Comes offmill scale·rust·oxides
Parts arecarbon steel·stainless steel
Also coversmill scale·oxide·pickling·black scale
Run it at2.5–10% v/v (typ. 5%)·ambient–50 °C, never above 60 in ultrasonics
Descale →

Acid mist rises sharply above 50 °C in ultrasonics; extraction is required.

Food industryImmersion / ultrasonic

Fats and food soils off food-contact equipment

Comes offfats·food soils·grease
Parts arestainless steel·glass·enamel·ceramic
Also coversfood·AQIS·food grade·kitchen·food contact
Run it at5–15% v/v (normal use 10%)·45–65 °C
FX Degreaser →

Hydrocarbons off oxygen service parts

Comes offhydrocarbon residues·oils
Parts arestainless steel·aluminium·copper alloys
Also coversoxygen·LOX·oxygen cleaning
Run it at3–15% (typ. 5%; 5% min on aluminium)·49–77 °C
AquaVantage 1990 GD →
Gas and oxygen serviceImmersion / ultrasonic

Hydrocarbon oils off oxygen system components

Comes offhydrocarbon oils·grease·particulate
Parts arestainless steel·copper alloys·brass·aluminium
Also coversoxygen·LOX·breathing air·regulator·cylinder valve
Run it at7–30% (typ. 10%)·54–77 °C
AquaVantage 815 GD →

Cutting oils and swarf off machined components

Comes offcutting oils·coolants·swarf·drawing compound
Parts aresteel·aluminium·brass
Also coversspray wash·parts washer·machined part·in-line washer
Run it at3–15% (typ. 5%)·49–82 °C
AquaVantage 1696 GD →
General manufacturingImmersion / ultrasonic

Rust and scale off steel before painting

Comes offrust·scale·grime
Parts arecarbon steel·cast iron
Also coversrust·pre-paint·derust·passivate
Run it at20% v/v + CoreKleen Plus 1–2% v/v·50–60 °C
CoreKleen HX →
General manufacturingImmersion / ultrasonic

Rust protection between process stages

Comes offapplied to clean parts, nothing to remove
Parts aresteel·cast iron
Also coversflash rust·rust prevention·between stages·in-process
Run it at2–5% v/v in the rinse tank·ambient–50 °C
Anti-Rust →

Ferrous only. Not for aluminium, zinc, magnesium, copper or brass, the ethanolamine content attacks copper alloys.

Heavy automotiveImmersion / ultrasonic

Baked carbon and soot off DPF and EGR parts

Comes offbaked carbon·soot·tenacious oils
Parts arestainless steel·steel
Also coversDPF·diesel particulate filter·EGR·EGR cooler·exhaust
Run it at5–30% (typ. 10%)·54–77 °C
AquaVantage 815 QR-NF →

Not suitable for sensitive materials. Keep copper, brass and plastics out of this bath.

Heavy machinery refurbishmentImmersion / ultrasonic

Paint and powder coat off housings and covers

Comes offpaint·powder coat·baked soils
Parts aresteel·cast iron·aluminium
Also covershousing·cover·painted steel·refurbishment
Run it at10% v/v of the mixed system·40–70 °C
AlloySystem →

Not safe on magnesium.

MarineImmersion / ultrasonic

Salt and carbon off marine engine heads

Comes offsalt deposits·oils·carbon·grime
Parts arealuminium·cast iron·steel
Also coversmarine engine·outboard·seawater·salt
Run it at10–20% v/v (typ. 15%)·40–60 °C
Desludge →

pH 13 in the bath. Zinc, galvanised, magnesium and soft solder are attacked.

Metal fabrication and weldingImmersion / ultrasonic

Weld flux and heat scale off fabrications

Comes offwelding flux·weld spatter·heat scale·oxides
Parts arestainless steel·carbon steel
Also coversweld·welding·flux·spatter·heat scale·weld tint
Run it at2.5–10% v/v (typ. 5%)·ambient–50 °C, never above 60 in ultrasonics
Descale →

On carbon steel and cast iron the base metal is attacked along with the scale, time-limit, rinse and neutralise. Bake hardened or high-tensile steel within 4 hours to relieve hydrogen embrittlement.

Mining and heavy plantImmersion / ultrasonic

Exhaust ash off DPFs on heavy plant

Comes offcalcium ash·mineral scale
Parts arecordierite·stainless steel
Also coversDPF·exhaust·ash·heavy plant·underground
Run it atneat, no dilution·ambient–50 °C
RegeniK →

Copper, brass and bronze can suffer stress-corrosion cracking. On carbon steel and cast iron, prolonged contact etches and flash-rusts, time-limit and dry promptly.

Mining and heavy plantImmersion / ultrasonic

Scale and red dirt out of radiator cores

Comes offscale·red dirt·mud·mineral deposits·coolant residue
Parts arealuminium·steel
Also coversradiator·radiator core·cooler core·charge air cooler·heat exchanger·red dirt·CAC
Run it at20% v/v + CoreKleen Plus 1–2% v/v·50–60 °C
CoreKleen HX →

Copper and brass cores are chelated on prolonged contact, time-limit the cycle and test a core first. Solder joints in older cores are the part to watch.

Mining and heavy plantImmersion / ultrasonic

Oil and road film off radiator internals

Comes offoil·grime·road film
Parts arealuminium·steel
Also coversradiator·cooler·internal surfaces·heat exchanger
Run it at10–20% v/v (typ. 15%)·40–60 °C
Desludge →

pH 13 in the bath. Zinc, galvanised, magnesium and soft solder are attacked, and copper and brass tarnish. Check what the core and headers are soldered with before immersion.

Mining and heavy plantImmersion / ultrasonic

White rust off zinc-plated parts

Comes offwhite rust·zinc oxide
Parts arezinc plating·galvanised steel
Also coverswhite rust·zinc·galvanised·plated
Run it at20% v/v + CoreKleen Plus 1–2% v/v·50–60 °C
CoreKleen HX →
Mould and tool cleaningImmersion / ultrasonic

Burned-on polymer off rubber moulds

Comes offburned-on polymer·release agent·carbon
Parts aresteel·cast iron
Also coversmould·tool·rubber mould·release agent
Run it at10–30% v/v (typ. 25%)·60–80 °C
MetalTek 100 →

Ferrous only.

Rust protection for steel held in store

Comes offapplied to clean parts, nothing to remove
Parts aresteel·cast iron
Also coversstorage·pre-plating·pre-painting·soak tank
Run it at2–5% v/v in the rinse tank·ambient–50 °C
Anti-Rust →

Ferrous only. Not for aluminium, zinc, magnesium, copper or brass, the ethanolamine content attacks copper alloys.

Fingerprints off vacuum and semiconductor parts

Comes offfingerprints·light oils·particulate
Parts arestainless steel·aluminium·copper alloys
Also coversvacuum·semiconductor·chamber part·high purity
Run it at3–15% (typ. 5%)·49–82 °C
AquaVantage 1696 GD →
PrintingImmersion / ultrasonic

Dried ink out of anilox roller cells

Comes offdried ink·burned-on polymer·lacquer
Parts aresteel·ceramic-coated steel
Also coversanilox·roller·print roller·ink
Run it at10–30% v/v (typ. 25%)·60–80 °C
MetalTek 100 →

Confirm the cell coating with the roller maker before immersion, caustic attacks some ceramic sealers.

RailImmersion / ultrasonic

Grease and road grime off traction motors

Comes offgrease·oils·road grime·carbon
Parts aresteel·copper windings
Also coverstraction motor·bogie·axle box
Run it at7–30% (typ. 10%)·54–77 °C
AquaVantage 815 GD →
Transport and railImmersion / ultrasonic

Scale and red dirt out of charge-air coolers

Comes offscale·mineral deposits·red dirt
Parts arealuminium·steel
Also coverscharge air cooler·intercooler·oil cooler·radiator
Run it at20% v/v + CoreKleen Plus 1–2% v/v·50–60 °C
CoreKleen HX →
Workshop and maintenanceImmersion / ultrasonic

Grease and shop dirt off workshop parts

Comes offlight grease·oils·shop dirt
Parts aresteel·cast iron·stainless steel·aluminium
Also coversworkshop·general purpose·bench·parts
Run it at5–15% v/v (normal use 10%)·45–65 °C
FX Degreaser →

Aluminium only inside the data sheet window, 5% v/v maximum, 50 °C maximum, 5 minutes, then rinse immediately.

Compatibility, dilution and temperature are taken from each product’s current technical data sheet. These are documented applications, not a substitute for a trial: confirm compatibility by testing under your own cleaning conditions. The compatibility matrix is the full picture, metal by metal.